Las Vegas Powder Coatings Blog

How Powder Coating Quality Is Checked: Film Thickness, Adhesion and Cure Tests

Las Vegas, NV · November 10, 2026

A powder-coated finish can look perfect and still have a problem you can't see. Is the coating thick enough? Is it stuck firmly to the metal? Did it fully cure in the oven? Finishers answer those questions with a few standard tests. Here's what each one checks, in plain language.

1. Film thickness: is there enough coating?

Powder makers list a recommended film thickness on their technical data sheets, usually in mils. A mil is one thousandth of an inch, or about 25 microns. For example, AkzoNobel's data sheet for Interpon A2201 recommends a film thickness of 2.0 to 2.5 mils.

After the part cures, thickness is measured with a handheld gauge that doesn't damage the finish. Gauge maker DeFelsko explains that these gauges use a magnetic principle on steel parts and an eddy current principle on aluminum and other metals, as long as the coating doesn't conduct electricity. ASTM D7091 is the standard practice for using them.

ASTM D7091 also points out that coating thickness can vary widely across a surface, so a single reading may not represent the whole part. That's why thickness is checked in more than one spot.

Cured thickness is what counts

DeFelsko notes that coating powders generally get thinner as they cure. Cured thickness targets are the values most often supplied by powder manufacturers and coating specifiers.

Rows of black-finished cylindrical metal parts laid out on a gray textured mat

2. Adhesion: is the coating stuck to the metal?

A common adhesion check is the tape test in ASTM D3359. Cuts are made through the coating, pressure-sensitive tape is pressed over the cuts and pulled off, and the result is rated by how much coating comes away with the tape.

The standard has two versions. Test Method B is meant for coatings under 5 mils (125 microns) thick, like the 2.0 to 2.5 mil example above. Test Method A is meant for coatings thicker than 5 mils.

ASTM says the tape test shows whether adhesion is adequate for the job. It doesn't tell apart higher levels of adhesion, which need more sophisticated test methods.

Good adhesion starts before any powder goes on, which is why surface preparation like sandblasting and chemical pretreatment matters.

3. Cure: did it fully cure in the oven?

As we covered in Powder Coating Cure Schedules Explained, powder has to reach the right temperature for the right amount of time to cure. A common way to check cure afterward is a solvent rub test.

In powder maker Vitracoat's solvent rub test method, a cotton swab soaked in MEK (methyl ethyl ketone) or a solvent blend is rubbed back and forth on the coating. One stroke forward and one stroke back counts as one "double rub." Vitracoat rates the results like this:

  • No cure: powder removed to bare metal
  • Partial or full cure: some film removal and softening, compared against a known sample
  • Cured coating: no effect on film appearance or gloss

The general solvent rub practice, ASTM D5402, does not set the solvent, the number of rubs or the expected result. Those details come from the powder supplier. Diamond Vogel also notes that not all coatings have the same solvent resistance, and that textured and metallic finishes can show some color transfer even when the film is intact.

Compare against a cured sample

Vitracoat says solvent rub results should always be compared with a known cured panel of the same powder. Without that comparison, it's only a solvent resistance test, not a cure test. The test should also be done with good ventilation.

What this means for your project

Our capabilities page lists the quality-control tools in our shop: DeFelsko mil thickness gauges, MEK swab testing and cross-hatch adhesion testing equipment.

If your parts need to meet a specific film thickness or test requirement, include it when you contact us about your project. For longer-term lab testing, see our guide to what ASTM B117 salt spray hours mean. You can also learn more about our powder coating services.

A finish can look perfect and still fall short. Thickness, adhesion and cure tests check what your eyes can't.

Check the data sheet

The powder's data sheet lists its recommended film thickness and test results.

Measure in several spots

Thickness can vary across a part, so one reading isn't enough.

Compare to a cured sample

A solvent rub only shows cure next to a known cured panel.

Sources

Have a spec your parts need to meet?

Contact us and tell us about your project.